Factors that influence machinability
| Factor | Effect |
|---|---|
| Hardness and strength | Higher cutting forces and temperatures; lower speeds |
| Work hardening | Surface hardens in front of the edge (austenitic stainless, nickel alloys) |
| Thermal conductivity | Low conductivity (titanium, nickel) concentrates heat at the edge |
| Abrasive phases | Carbides and inclusions wear tools (tool steels, cast iron, Ti-stabilised stainless) |
| Ductility | Long stringy chips and burrs (pure copper, low-carbon steel, aluminium 1xxx/5xxx) |
| Free-machining additions | Sulphur, lead, bismuth or selenium improve chip breaking |
| Microstructure / condition | Annealed vs. quenched & tempered changes everything |
Machinability ratings
Traditional ratings compare materials with a reference free-cutting steel (e.g. AISI 1212 = 100 %). They are useful for orientation but depend on test conditions and do not translate directly to modern carbide tooling. Our materials reference uses a simple A–D scale instead.
Difficult materials — practical approach
- Stainless steels: sharp positive geometry, constant feed (never rub), adequate depth to cut below the work-hardened layer.
- Titanium: low cutting speeds, high-pressure coolant, sharp tools, rigid set-up; avoid dwell.
- Nickel alloys: ceramic or carbide tools with careful speed control, frequent edge changes, trochoidal strategies.
- Hardened steels: CBN and ceramic tools for hard turning; grinding for tightest tolerances.
- Plastics: sharp polished tools, low clamping forces, allow for thermal expansion; anneal stock for tight tolerances.