Drawings from different regions use different material systems. Cross-referencing is necessary — but grades that look alike are not automatically interchangeable.

Three categories

Equivalent
the same standardised alloy registered in another system (e.g. EN AW-7075 and AA 7075). Still check temper, product standard and certificate requirements.
Comparable
similar chemistry and use, but composition ranges and mechanical requirements differ (e.g. 1.4404 and AISI 316L). Usually acceptable after review.
Closest substitute
nearest practical alternative when no direct counterpart exists (e.g. EN AW-6082 and AA 6061). Requires engineering approval.

Substitution checklist

  • Chemical composition limits, including restricted elements (lead, sulphur, boron).
  • Mechanical properties in the delivery condition and the relevant section size.
  • Heat-treatment response and required hardness.
  • Corrosion behaviour in the actual environment.
  • Certificate type (EN 10204 3.1 / 3.2) and product standard.
  • Customer approval documented before production.

Cross-reference table

EN / NameW.-Nr. / EN no.US (AISI / UNS / ASTM)RelationMachinabilityDensity g/cm³Typical use / notes
S235JR
Carbon & free-cutting steels
1.0038ASTM A36ComparableB – good7.85General structural steel for brackets, plates and welded frames. Machines readily but can tear on finishing passes.
S355J2
Carbon & free-cutting steels
1.0577ASTM A572 Gr. 50ComparableB – good7.85Higher-strength structural steel for frames, bases and welded machine structures.
C45 / C45E
Carbon & free-cutting steels
1.0503 / 1.1191AISI 1045 · UNS G10450ComparableB – good7.85Medium-carbon steel for shafts, pins and gears; can be flame or induction hardened.
11SMn30
Carbon & free-cutting steels
1.0715AISI 1215 · UNS G12150ComparableA – very good7.85Free-cutting steel with sulphur for high-volume turned parts; limited weldability and case-hardening response.
11SMnPb30
Carbon & free-cutting steels
1.0718AISI 12L14 · UNS G12144ComparableA – very good7.85Leaded free-cutting steel with excellent chip breaking. Check RoHS / REACH and customer lead restrictions.
16MnCr5
Alloy & case-hardening steels
1.7131AISI 5115 · UNS G51150ComparableB – good7.85Case-hardening steel for gears, pins and shafts that need a hard surface and tough core.
20MnCr5
Alloy & case-hardening steels
1.7147AISI 5120Closest substituteB – good7.85Case-hardening steel for more heavily loaded gears and shafts. US grades differ in Cr/Mn content.
42CrMo4
Alloy & case-hardening steels
1.7225AISI 4140 · UNS G41400ComparableC – moderate7.85Quenched-and-tempered alloy steel for highly loaded shafts, studs and hydraulic parts. Machinability falls as hardness rises.
34CrNiMo6
Alloy & case-hardening steels
1.6582AISI 4340 · UNS G43400ComparableC – moderate7.85High-toughness Ni-Cr-Mo steel for heavily stressed shafts, crankshafts and defence components.
100Cr6
Alloy & case-hardening steels
1.3505AISI 52100 · UNS G52986ComparableC – moderate7.81Through-hardening bearing steel; usually machined soft-annealed, then hardened and ground.
X153CrMoV12
Tool steels
1.2379AISI D2 · UNS T30402ComparableD – difficult7.7High-carbon high-chromium cold-work tool steel. Abrasive carbides — machined annealed, finished by grinding or hard milling.
X40CrMoV5-1
Tool steels
1.2344AISI H13 · UNS T20813ComparableC – moderate7.8Hot-work tool steel for dies, inserts and moulds; often pre-hardened for direct machining.
90MnCrV8
Tool steels
1.2842AISI O2 · UNS T31502ComparableC – moderate7.85Oil-hardening cold-work tool steel for gauges, punches and wear parts.
40CrMnNiMo8-6-4
Tool steels
1.2738AISI P20 (+Ni)Closest substituteC – moderate7.85Pre-hardened plastic-mould steel (typically ~ 280–325 HB as supplied). P20 variants differ in nickel content.
X5CrNi18-10
Stainless steels
1.4301AISI 304 · UNS S30400ComparableC – moderate7.9Standard austenitic stainless steel. Work-hardens; requires sharp tools and continuous feed.
X2CrNi18-9
Stainless steels
1.4307AISI 304L · UNS S30403ComparableC – moderate7.9Low-carbon 304L for welded assemblies.
X8CrNiS18-9
Stainless steels
1.4305AISI 303 · UNS S30300ComparableB – good7.9Free-machining stainless with sulphur — good for turned parts, lower corrosion resistance and poor weldability.
X5CrNiMo17-12-2
Stainless steels
1.4401AISI 316 · UNS S31600ComparableC – moderate8Mo-alloyed austenitic stainless for chloride and chemical exposure.
X2CrNiMo17-12-2
Stainless steels
1.4404AISI 316L · UNS S31603ComparableC – moderate8Low-carbon 316L; the common choice for pharmaceutical, food and marine parts.
X6CrNiMoTi17-12-2
Stainless steels
1.4571AISI 316Ti · UNS S31635ComparableC – moderate8Ti-stabilised 316 grade, common in Germany for welded process equipment. Titanium carbonitrides increase tool wear.
X20Cr13
Stainless steels
1.4021AISI 420 · UNS S42000ComparableB – good7.7Martensitic stainless for pump shafts and valve parts; hardenable.
X17CrNi16-2
Stainless steels
1.4057AISI 431 · UNS S43100ComparableC – moderate7.7Martensitic Cr-Ni stainless with higher toughness and corrosion resistance than 420; used for shafts and marine fittings.
X5CrNiCuNb16-4
Stainless steels
1.454217-4PH (630) · UNS S17400ComparableC – moderate7.8Precipitation-hardening stainless. Usually machined in condition A or H1150 and aged afterwards; ageing causes slight dimensional change.
X2CrNiMoN22-5-3
Stainless steels
1.44622205 · UNS S32205 / S31803ComparableD – difficult7.8Duplex stainless with high strength and pitting resistance. Tough to machine: rigid set-ups and lower cutting speeds.
EN AW-6061 (AlMg1SiCu)
Aluminium alloys
3.3211 (former)AA 6061 · UNS A96061EquivalentB – good2.7Versatile heat-treatable alloy (T6/T651). Good machinability and anodising response.
EN AW-6082 (AlSi1MgMn)
Aluminium alloys
3.2315 (former)AA 6061 / 6351Closest substituteB – good2.7The standard European structural extrusion alloy; often substituted by 6061 in North America.
EN AW-7075 (AlZn5,5MgCu)
Aluminium alloys
3.4365 (former)AA 7075 · UNS A97075EquivalentB – good2.81High-strength Al-Zn alloy for aerospace and motorsport. Not weldable by conventional methods.
EN AW-2024 (AlCu4Mg1)
Aluminium alloys
3.1355 (former)AA 2024 · UNS A92024EquivalentB – good2.78High fatigue strength Al-Cu alloy; poor corrosion resistance unless clad or protected.
EN AW-2007 (AlCu4PbMgMn)
Aluminium alloys
3.1645 (former)AA 2011Closest substituteA – very good2.85Leaded free-machining aluminium for high-volume turned parts; check lead restrictions.
EN AW-5083 (AlMg4,5Mn0,7)
Aluminium alloys
3.3547 (former)AA 5083 · UNS A95083EquivalentC – moderate2.66Non-heat-treatable marine alloy. Gummy chips; needs sharp, polished tools.
CuZn39Pb3
Copper alloys
CW614NC38500ComparableA – very good8.47Leaded free-cutting brass — benchmark for machinability. Lead content may be restricted (RoHS exemptions, drinking-water rules).
CuZn40Pb2
Copper alloys
CW617NC37700ComparableA – very good8.43Leaded brass for hot stampings and turned fittings.
Cu-ETP
Copper alloys
CW004AC11000ComparableD – difficult8.93High-conductivity copper for busbars and electrical contacts. Soft and gummy; burr control is critical.
CuSn8
Copper alloys
CW453KC52100ComparableC – moderate8.8Phosphor bronze for bushings, springs and bearing parts.
CuAl10Ni5Fe4
Copper alloys
CW307GC63000ComparableC – moderate7.6Nickel-aluminium bronze with excellent seawater resistance; used for propeller, pump and valve parts.
Ti Grade 2
Titanium
3.7035ASTM B348 Gr. 2 · UNS R50400EquivalentC – moderate4.51Commercially pure titanium — corrosion resistant and ductile. Low thermal conductivity concentrates heat at the edge.
Ti-6Al-4V (Grade 5)
Titanium
3.7165ASTM B348 Gr. 5 · UNS R56400EquivalentD – difficult4.43The most widely used titanium alloy. Needs low cutting speeds, high-pressure coolant and rigid fixturing.
NiCr22Mo9Nb (Alloy 625)
Nickel alloys
2.4856UNS N06625EquivalentD – difficult8.44Ni-Cr-Mo superalloy for corrosive and high-temperature service. Severe work hardening.
NiCr19NbMo (Alloy 718)
Nickel alloys
2.4668UNS N07718EquivalentD – difficult8.19Precipitation-hardening superalloy for turbine and oil-and-gas parts; usually machined solution-annealed or aged depending on the drawing.
NiCu30Fe (Alloy 400)
Nickel alloys
2.4360UNS N04400EquivalentC – moderate8.8Ni-Cu alloy with excellent seawater resistance; gummy, prone to built-up edge.
EN-GJL-250
Cast irons
EN-JL1040ASTM A48 Class 35/40ComparableA – very good7.2Grey cast iron for housings and machine bases; short chips, abrasive, dust extraction recommended.
EN-GJS-400-15
Cast irons
EN-JS1030ASTM A536 60-40-18ComparableB – good7.1Ductile (nodular) iron for housings, hubs and brackets.
EN-GJS-700-2
Cast irons
EN-JS1070ASTM A536 100-70-03ComparableC – moderate7.2High-strength pearlitic ductile iron for gears and heavily loaded parts.
POM-C (acetal copolymer)
Engineering plastics
———A – very good1.41Dimensionally stable acetal for bushings, gears and fixtures; easy to machine to tight tolerances.
POM-H (acetal homopolymer)
Engineering plastics
———A – very good1.42Acetal homopolymer with slightly higher strength and stiffness; may show centreline porosity in thick stock.
PA 6 / PA 66
Engineering plastics
———B – good1.14Tough polyamides for wear parts and rollers. Absorb moisture — allow for dimensional change.
PET (semi-crystalline)
Engineering plastics
———A – very good1.39Semi-crystalline PET with low moisture uptake and good dimensional stability.
PEEK
Engineering plastics
———B – good1.3High-performance polymer for high temperatures and chemical exposure; also medical grades. Anneal for tight tolerances.
PTFE
Engineering plastics
———C – moderate2.17Very low friction and chemical resistance; soft, creeps and has high thermal expansion.
PE-UHMW
Engineering plastics
———C – moderate0.93Wear-resistant, low-friction polyethylene for guides and food conveyor parts; high thermal expansion.
Relation: Equivalent = the same standardised alloy under another designation system; Comparable = similar composition, but chemical and mechanical limits differ and must be checked; Closest substitute = nearest practical alternative, not interchangeable without engineering approval. Machinability is a qualitative ranking for orientation only — condition, hardness and the specific heat or batch strongly affect it. Densities are nominal values.
Responsibility

This table supports engineering judgement; it does not replace it. Any material substitution is proposed in writing and implemented only with the customer's approval.

Enquiry

Have a drawing to review?

Send your 2D drawing and 3D model with quantities, material and required documents. An engineer reviews manufacturability, tolerances and inspection before quoting.

What to include in your enquiry