MACHINING.TRPrecision Machining. Engineered in Turkey.
Turning insert cutting a steel shaft
  1. Home
  2. Quality
  3. Defects Library

Quality

Machining defects library

Most machining defects have well-known causes. This library summarises what you see, why it happens, how to correct it and how to prevent it.

Defects

Chatter marks01
What you see
Regular wavy pattern on walls or floors, loud vibration, poor finish, chipped edges.
Likely causes
Long tool overhang, thin walls, weak workholding, spindle speed in an unstable range, too large radial engagement.
Corrective actions
Shorten overhang, change spindle speed by 5–15 %, reduce ae, use variable-pitch cutters, add support or damping.
Prevention & detection
Review stick-out and wall thickness at CAM stage; listen and inspect first part; check finish against drawing.
Burrs02
What you see
Raised material at edges, hole exits and cross-holes; sharp edges that cut fingers or block assembly.
Likely causes
Ductile material, worn edges, exit strategy, negative geometry, no deburring operation planned.
Corrective actions
Sharp positive tools, climb milling on exit edges, chamfer passes in program, dedicated deburring tools for cross-holes.
Prevention & detection
Specify edge condition per ISO 13715 on drawing; visual and tactile check of every edge class.
Built-up edge (BUE)03
What you see
Torn, smeared surface; material welded on the cutting edge; size drift.
Likely causes
Low cutting speed in sticky materials (aluminium, low-carbon and stainless steel), uncoated or dull edges, poor lubrication.
Corrective actions
Increase cutting speed, use polished or suitable coated grades, improve coolant concentration and delivery.
Prevention & detection
Monitor edge condition at tool change; check roughness on first parts of each batch.
Dimensional drift during a batch04
What you see
Parts start in tolerance and gradually move toward a limit.
Likely causes
Tool wear, machine warm-up and thermal growth, coolant temperature change.
Corrective actions
Wear offsets based on measurement, warm-up cycle, in-process probing, scheduled tool life.
Prevention & detection
SPC on critical features, defined measurement frequency, control charts.
Taper on turned diameters05
What you see
Diameter differs from one end to the other.
Likely causes
Deflection of slender parts, tailstock misalignment, tool wear along a long cut, machine geometry.
Corrective actions
Support with tailstock or steady rest, balanced roughing, finishing pass with constant engagement, check alignment.
Prevention & detection
Measure at both ends and mid-length; L/D ratio review at planning stage.
Out-of-round / lobing06
What you see
Roundness error; three-lobed shape in thin rings or bores.
Likely causes
Excessive chuck pressure, thin-walled parts, residual stress, spindle run-out.
Corrective actions
Reduce clamping force for finishing, soft jaws bored to size, pie jaws, stress-relieve before finishing.
Prevention & detection
Roundness measurement (not only two-point diameter), clamping strategy defined in process plan.
Poor surface finish07
What you see
Roughness above specification, visible feed marks or tearing.
Likely causes
Feed too high for nose radius, worn tool, vibration, unsuitable cutting speed, chip re-cutting.
Corrective actions
Optimise feed vs. nose radius, wiper inserts, fresh edge for finishing, chip evacuation with coolant or air.
Prevention & detection
Roughness measurement with defined cut-off; compare with theoretical Rt.
Thread defects08
What you see
Gauge does not go in or no-go gauge enters; torn flanks, broken taps.
Likely causes
Wrong pre-drill size, chip packing in blind holes, worn taps, incorrect pitch-synchronous feed, wrong tolerance class.
Corrective actions
Correct tap-drill diameter, spiral-flute taps for blind holes, thread milling for difficult materials, verify class (6H/6g).
Prevention & detection
GO/NO-GO thread gauges at defined frequency; check thread depth.
Position errors between features09
What you see
Holes or features correct in size but wrongly located relative to datums.
Likely causes
Re-clamping between operations, incorrect datum set-up, fixture wear, thermal effects.
Corrective actions
Machine related features in one set-up, datum-based fixtures, probing of datums before cutting.
Prevention & detection
CMM measurement against the datum reference frame defined on the drawing.
Flatness / distortion after unclamping10
What you see
Plate parts rock on a surface plate; dimensions change after release from the vice.
Likely causes
Residual stresses in raw material, unbalanced material removal, clamping distortion, heat.
Corrective actions
Rough both sides, release and re-clamp before finishing, stress-relieved material, symmetrical removal.
Prevention & detection
Flatness check after unclamping; use stress-relieved plate (e.g. T651) where specified.
Tool breakage11
What you see
Sudden failure, scrapped part, broken tool fragments in features.
Likely causes
Excessive chip load, chip packing, hard spots, wrong grade, collisions.
Corrective actions
Correct feeds, peck cycles, chip evacuation, tool-path smoothing, tool breakage detection.
Prevention & detection
Program simulation, first-part supervision, tool life management.
Hard-spot and scale damage12
What you see
Rapid edge failure at certain locations; visible scale or skin on stock.
Likely causes
Casting or forging skin, sand inclusions, local hardness from flame cutting or welding.
Corrective actions
First pass below the skin with tough grade, lower speed, remove heat-affected zones.
Prevention & detection
Incoming inspection of castings/forgings; hardness check.
Heat discolouration13
What you see
Blue or straw colours on steel or titanium; changed surface properties.
Likely causes
Excessive cutting speed, worn tools, insufficient coolant, grinding burn.
Corrective actions
Reduce speed, fresh tools, improve coolant flow, correct grinding wheel and dressing.
Prevention & detection
Visual inspection; etch inspection for grinding burn where specified.
Wrong material or mixed stock14
What you see
Unexpected chip behaviour or hardness; certificate does not match marking.
Likely causes
Poor bar identification, mixed remnants, supplier error.
Corrective actions
Quarantine, PMI or chemical analysis, trace to heat number.
Prevention & detection
Heat-number traceability from bar to part, EN 10204 3.1 certificates, PMI where required.
Surface damage in handling15
What you see
Dents, scratches, edge damage on finished parts.
Likely causes
Parts touching in bins, unsuitable packaging, rough handling between operations.
Corrective actions
Separators, dedicated trays, protective caps for threads and seal faces.
Prevention & detection
Defined packaging specification; final visual inspection before packing.
Corrosion after machining16
What you see
Rust spots on steel parts in storage or transit; staining on stainless.
Likely causes
Coolant residue, humidity, contact with carbon-steel tools or swarf on stainless.
Corrective actions
Cleaning, corrosion inhibitor, VCI packaging, segregated tooling and brushes for stainless.
Prevention & detection
Defined cleaning and preservation step; packing inspection for export shipments.

Using the library

Defects are rarely caused by a single factor. Root-cause analysis looks at the 6M — machine, method, material, measurement, man and environment (mother nature) — and verifies the fix on the next parts. Use this library as a checklist, not as a replacement for analysis.

Enquiry

Have a drawing to review?

Send your 2D drawing and 3D model with quantities, material and required documents. An engineer reviews manufacturability, tolerances and inspection before quoting.

What to include in your enquiry