How to use this reference
Filter by group or search for any designation — EN name, material number, AISI/UNS grade or application. The relation column tells you whether a US designation is the same alloy, a comparable one, or only the closest substitute. The machinability letter is qualitative guidance relative to other materials in the table.
| EN / Name | W.-Nr. / EN no. | US (AISI / UNS / ASTM) | Relation | Machinability | Density g/cm³ | Typical use / notes |
|---|---|---|---|---|---|---|
| S235JR Carbon & free-cutting steels | 1.0038 | ASTM A36 | Comparable | B – good | 7.85 | General structural steel for brackets, plates and welded frames. Machines readily but can tear on finishing passes. |
| S355J2 Carbon & free-cutting steels | 1.0577 | ASTM A572 Gr. 50 | Comparable | B – good | 7.85 | Higher-strength structural steel for frames, bases and welded machine structures. |
| C45 / C45E Carbon & free-cutting steels | 1.0503 / 1.1191 | AISI 1045 · UNS G10450 | Comparable | B – good | 7.85 | Medium-carbon steel for shafts, pins and gears; can be flame or induction hardened. |
| 11SMn30 Carbon & free-cutting steels | 1.0715 | AISI 1215 · UNS G12150 | Comparable | A – very good | 7.85 | Free-cutting steel with sulphur for high-volume turned parts; limited weldability and case-hardening response. |
| 11SMnPb30 Carbon & free-cutting steels | 1.0718 | AISI 12L14 · UNS G12144 | Comparable | A – very good | 7.85 | Leaded free-cutting steel with excellent chip breaking. Check RoHS / REACH and customer lead restrictions. |
| 16MnCr5 Alloy & case-hardening steels | 1.7131 | AISI 5115 · UNS G51150 | Comparable | B – good | 7.85 | Case-hardening steel for gears, pins and shafts that need a hard surface and tough core. |
| 20MnCr5 Alloy & case-hardening steels | 1.7147 | AISI 5120 | Closest substitute | B – good | 7.85 | Case-hardening steel for more heavily loaded gears and shafts. US grades differ in Cr/Mn content. |
| 42CrMo4 Alloy & case-hardening steels | 1.7225 | AISI 4140 · UNS G41400 | Comparable | C – moderate | 7.85 | Quenched-and-tempered alloy steel for highly loaded shafts, studs and hydraulic parts. Machinability falls as hardness rises. |
| 34CrNiMo6 Alloy & case-hardening steels | 1.6582 | AISI 4340 · UNS G43400 | Comparable | C – moderate | 7.85 | High-toughness Ni-Cr-Mo steel for heavily stressed shafts, crankshafts and defence components. |
| 100Cr6 Alloy & case-hardening steels | 1.3505 | AISI 52100 · UNS G52986 | Comparable | C – moderate | 7.81 | Through-hardening bearing steel; usually machined soft-annealed, then hardened and ground. |
| X153CrMoV12 Tool steels | 1.2379 | AISI D2 · UNS T30402 | Comparable | D – difficult | 7.7 | High-carbon high-chromium cold-work tool steel. Abrasive carbides — machined annealed, finished by grinding or hard milling. |
| X40CrMoV5-1 Tool steels | 1.2344 | AISI H13 · UNS T20813 | Comparable | C – moderate | 7.8 | Hot-work tool steel for dies, inserts and moulds; often pre-hardened for direct machining. |
| 90MnCrV8 Tool steels | 1.2842 | AISI O2 · UNS T31502 | Comparable | C – moderate | 7.85 | Oil-hardening cold-work tool steel for gauges, punches and wear parts. |
| 40CrMnNiMo8-6-4 Tool steels | 1.2738 | AISI P20 (+Ni) | Closest substitute | C – moderate | 7.85 | Pre-hardened plastic-mould steel (typically ~ 280–325 HB as supplied). P20 variants differ in nickel content. |
| X5CrNi18-10 Stainless steels | 1.4301 | AISI 304 · UNS S30400 | Comparable | C – moderate | 7.9 | Standard austenitic stainless steel. Work-hardens; requires sharp tools and continuous feed. |
| X2CrNi18-9 Stainless steels | 1.4307 | AISI 304L · UNS S30403 | Comparable | C – moderate | 7.9 | Low-carbon 304L for welded assemblies. |
| X8CrNiS18-9 Stainless steels | 1.4305 | AISI 303 · UNS S30300 | Comparable | B – good | 7.9 | Free-machining stainless with sulphur — good for turned parts, lower corrosion resistance and poor weldability. |
| X5CrNiMo17-12-2 Stainless steels | 1.4401 | AISI 316 · UNS S31600 | Comparable | C – moderate | 8 | Mo-alloyed austenitic stainless for chloride and chemical exposure. |
| X2CrNiMo17-12-2 Stainless steels | 1.4404 | AISI 316L · UNS S31603 | Comparable | C – moderate | 8 | Low-carbon 316L; the common choice for pharmaceutical, food and marine parts. |
| X6CrNiMoTi17-12-2 Stainless steels | 1.4571 | AISI 316Ti · UNS S31635 | Comparable | C – moderate | 8 | Ti-stabilised 316 grade, common in Germany for welded process equipment. Titanium carbonitrides increase tool wear. |
| X20Cr13 Stainless steels | 1.4021 | AISI 420 · UNS S42000 | Comparable | B – good | 7.7 | Martensitic stainless for pump shafts and valve parts; hardenable. |
| X17CrNi16-2 Stainless steels | 1.4057 | AISI 431 · UNS S43100 | Comparable | C – moderate | 7.7 | Martensitic Cr-Ni stainless with higher toughness and corrosion resistance than 420; used for shafts and marine fittings. |
| X5CrNiCuNb16-4 Stainless steels | 1.4542 | 17-4PH (630) · UNS S17400 | Comparable | C – moderate | 7.8 | Precipitation-hardening stainless. Usually machined in condition A or H1150 and aged afterwards; ageing causes slight dimensional change. |
| X2CrNiMoN22-5-3 Stainless steels | 1.4462 | 2205 · UNS S32205 / S31803 | Comparable | D – difficult | 7.8 | Duplex stainless with high strength and pitting resistance. Tough to machine: rigid set-ups and lower cutting speeds. |
| EN AW-6061 (AlMg1SiCu) Aluminium alloys | 3.3211 (former) | AA 6061 · UNS A96061 | Equivalent | B – good | 2.7 | Versatile heat-treatable alloy (T6/T651). Good machinability and anodising response. |
| EN AW-6082 (AlSi1MgMn) Aluminium alloys | 3.2315 (former) | AA 6061 / 6351 | Closest substitute | B – good | 2.7 | The standard European structural extrusion alloy; often substituted by 6061 in North America. |
| EN AW-7075 (AlZn5,5MgCu) Aluminium alloys | 3.4365 (former) | AA 7075 · UNS A97075 | Equivalent | B – good | 2.81 | High-strength Al-Zn alloy for aerospace and motorsport. Not weldable by conventional methods. |
| EN AW-2024 (AlCu4Mg1) Aluminium alloys | 3.1355 (former) | AA 2024 · UNS A92024 | Equivalent | B – good | 2.78 | High fatigue strength Al-Cu alloy; poor corrosion resistance unless clad or protected. |
| EN AW-2007 (AlCu4PbMgMn) Aluminium alloys | 3.1645 (former) | AA 2011 | Closest substitute | A – very good | 2.85 | Leaded free-machining aluminium for high-volume turned parts; check lead restrictions. |
| EN AW-5083 (AlMg4,5Mn0,7) Aluminium alloys | 3.3547 (former) | AA 5083 · UNS A95083 | Equivalent | C – moderate | 2.66 | Non-heat-treatable marine alloy. Gummy chips; needs sharp, polished tools. |
| CuZn39Pb3 Copper alloys | CW614N | C38500 | Comparable | A – very good | 8.47 | Leaded free-cutting brass — benchmark for machinability. Lead content may be restricted (RoHS exemptions, drinking-water rules). |
| CuZn40Pb2 Copper alloys | CW617N | C37700 | Comparable | A – very good | 8.43 | Leaded brass for hot stampings and turned fittings. |
| Cu-ETP Copper alloys | CW004A | C11000 | Comparable | D – difficult | 8.93 | High-conductivity copper for busbars and electrical contacts. Soft and gummy; burr control is critical. |
| CuSn8 Copper alloys | CW453K | C52100 | Comparable | C – moderate | 8.8 | Phosphor bronze for bushings, springs and bearing parts. |
| CuAl10Ni5Fe4 Copper alloys | CW307G | C63000 | Comparable | C – moderate | 7.6 | Nickel-aluminium bronze with excellent seawater resistance; used for propeller, pump and valve parts. |
| Ti Grade 2 Titanium | 3.7035 | ASTM B348 Gr. 2 · UNS R50400 | Equivalent | C – moderate | 4.51 | Commercially pure titanium — corrosion resistant and ductile. Low thermal conductivity concentrates heat at the edge. |
| Ti-6Al-4V (Grade 5) Titanium | 3.7165 | ASTM B348 Gr. 5 · UNS R56400 | Equivalent | D – difficult | 4.43 | The most widely used titanium alloy. Needs low cutting speeds, high-pressure coolant and rigid fixturing. |
| NiCr22Mo9Nb (Alloy 625) Nickel alloys | 2.4856 | UNS N06625 | Equivalent | D – difficult | 8.44 | Ni-Cr-Mo superalloy for corrosive and high-temperature service. Severe work hardening. |
| NiCr19NbMo (Alloy 718) Nickel alloys | 2.4668 | UNS N07718 | Equivalent | D – difficult | 8.19 | Precipitation-hardening superalloy for turbine and oil-and-gas parts; usually machined solution-annealed or aged depending on the drawing. |
| NiCu30Fe (Alloy 400) Nickel alloys | 2.4360 | UNS N04400 | Equivalent | C – moderate | 8.8 | Ni-Cu alloy with excellent seawater resistance; gummy, prone to built-up edge. |
| EN-GJL-250 Cast irons | EN-JL1040 | ASTM A48 Class 35/40 | Comparable | A – very good | 7.2 | Grey cast iron for housings and machine bases; short chips, abrasive, dust extraction recommended. |
| EN-GJS-400-15 Cast irons | EN-JS1030 | ASTM A536 60-40-18 | Comparable | B – good | 7.1 | Ductile (nodular) iron for housings, hubs and brackets. |
| EN-GJS-700-2 Cast irons | EN-JS1070 | ASTM A536 100-70-03 | Comparable | C – moderate | 7.2 | High-strength pearlitic ductile iron for gears and heavily loaded parts. |
| POM-C (acetal copolymer) Engineering plastics | — | — | — | A – very good | 1.41 | Dimensionally stable acetal for bushings, gears and fixtures; easy to machine to tight tolerances. |
| POM-H (acetal homopolymer) Engineering plastics | — | — | — | A – very good | 1.42 | Acetal homopolymer with slightly higher strength and stiffness; may show centreline porosity in thick stock. |
| PA 6 / PA 66 Engineering plastics | — | — | — | B – good | 1.14 | Tough polyamides for wear parts and rollers. Absorb moisture — allow for dimensional change. |
| PET (semi-crystalline) Engineering plastics | — | — | — | A – very good | 1.39 | Semi-crystalline PET with low moisture uptake and good dimensional stability. |
| PEEK Engineering plastics | — | — | — | B – good | 1.3 | High-performance polymer for high temperatures and chemical exposure; also medical grades. Anneal for tight tolerances. |
| PTFE Engineering plastics | — | — | — | C – moderate | 2.17 | Very low friction and chemical resistance; soft, creeps and has high thermal expansion. |
| PE-UHMW Engineering plastics | — | — | — | C – moderate | 0.93 | Wear-resistant, low-friction polyethylene for guides and food conveyor parts; high thermal expansion. |
Choosing a material
- Start from function: strength, stiffness, wear, corrosion, temperature, conductivity, weight, regulatory requirements.
- Then consider supply: standard bar and plate sizes, certification and lead time. A common grade in stock beats a rare one that must be melted.
- Then consider manufacturing: machinability, heat treatment, coating and joining.
Designations from different systems rarely define exactly the same chemistry, mechanical properties and test requirements. Even where an alloy is "the same", the delivery condition and certificate requirements must match your specification. See material equivalents.
Material groups at a glance
| Group | Strengths | Machining considerations |
|---|---|---|
| Carbon & free-cutting steels | Low cost, good machinability | Free-cutting grades limit welding and hardening |
| Alloy steels | High strength after heat treatment | Machine soft, finish after hardening if needed |
| Stainless steels | Corrosion resistance | Work hardening, heat, built-up edge |
| Aluminium alloys | Light, fast to machine | Burrs, distortion of thin walls |
| Copper alloys | Conductivity, bearing properties | Lead restrictions; pure copper is gummy |
| Titanium | Strength-to-weight, biocompatibility | Low speeds, heat concentration |
| Nickel alloys | Heat and corrosion resistance | Severe work hardening, tool wear |
| Engineering plastics | Low weight, insulation, chemical resistance | Thermal expansion, creep, stress relief |